Resumen
The corrosion behavior of type 304L and type 316L austenitic stainless steels, produced by powder metallurgy, when exposed to a ferric chloride solution was studied. The exposures were conducted according to ASTM G48-76, Method A. The influence of ferric chloride concentration and exposure temperature on the corrosion kinetics of these materials was evaluated. A mechanism is proposed to explain the associated morphology observed in the microstructures produced after exposure of these P/M alloys to the aggressive medium. © 1995.